Semi-Solid X-Ray CT Inspection for Cell Quality
I have spent the better part of a decade on semi-solid cell lines, and the one tool I never argue about is X-ray inspection. A semi-solid cell hides its worst problems inside an opaque pouch or aluminum can. Gel electrolyte, a composite cathode, and a graphite or lithium-metal anode all sit behind a foil stack that no camera can see. When a customer returns a pack with unexplained capacity loss, the root cause is almost always internal. In this guide I share how we use 2D radiography and computed tomography to find those defects, which settings actually matter, and how the data feeds a lot release decision. The goal is not inspection for its own sake. It is making a defensible call on every cell we ship.

What X-Ray and CT Reveal Inside a Semi-Solid Cell
X-ray imaging works because density and atomic number change how a beam is absorbed as it passes through the cell. Heavy elements such as copper tab welds and aluminum tabs attenuate strongly and show up bright on the detector. The electrode stack, separator, and gel electrolyte are far less dense and appear as softer gray bands. That contrast is exactly what we need to judge stack alignment without opening the cell. A semi-solid design adds a wrinkle: the gel phase is not as uniform as a liquid fill, so local density variation can look like a defect if you do not know the process baseline.
Two-dimensional radiography projects the whole thickness onto one flat image. It is fast, cheap, and ideal for checking tab placement, foil alignment, and gross foreign material. Computed tomography rotates the cell and reconstructs a three-dimensional volume from hundreds of projections. With a voxel size in the 30 to 80 micrometer range, a CT scan resolves pores, electrode folds, and separator creep that a flat image simply overlaps. For a semi-solid cell, where the electrolyte is partially immobilized, those internal features strongly influence ionic transport and long-term capacity retention. I treat 2D as the screening gate and CT as the diagnostic tool we reach for when screening flags something unusual.
The Defects That Actually Matter
After reviewing thousands of scans, the defects worth acting on fall into a short list. Electrode misalignment is the most common. If the anode overhangs the cathode unevenly, lithium plating can start at the exposed edge during fast charge, and the cell loses capacity far earlier than the model predicts. Separator folds and wrinkles are next. In a semi-solid stack the gel layer adds stiffness, so a fold introduced during stacking does not relax on its own; it stays as a hard crease that can bridge the electrodes under compression.
Foreign material is the defect that keeps quality managers awake. A fragment of metal from a slitting blade or a flake of dried slurry inside the pouch is invisible until it causes an internal short. X-ray catches dense particles reliably, while CT localizes them in three dimensions so we can trace which process step introduced them. Internal voids and poor wetting also show up clearly. We have correlated low-density regions in the electrode with higher impedance measured later on a reference cell. Tab welding is a special case: we pair X-ray inspection with a torque and pull check on a sample basis, because a weld can look sound in projection yet fail mechanically. None of these defects are unique to semi-solid chemistry, but the partial gel phase makes a few of them, especially voids and folds, harder to detect by electrical tests alone.
Choosing 2D Radiography vs 3D CT
The decision is usually about throughput, not capability. An in-line 2D system can inspect every cell at the line rate because exposure times are short and the image analysis is simple. We use it as a 100 percent gate for tab position and gross alignment on semi-solid pouch and prismatic cells. It will not tell you the depth of a void or which layer a fold sits in, but it will reliably reject a cell that is clearly out of spec.
CT is slower. A full scan with a few hundred projections can take minutes, so we apply it to a statistical sample and to any cell the 2D gate flags. The return is a volume you can slice in any plane, measure porosity in a defined region of interest, and compare against a known-good reference. I recommend a tiered approach. Screen every unit with 2D, scan a fixed sample with CT each shift to confirm the process baseline, and run full CT on every failure returned from the field. That structure gives you both coverage and diagnosis without turning the inspection room into a bottleneck.
Where X-Ray Fluorescence Fits
One related tool is worth mentioning. X-ray fluorescence, or XRF, measures elemental loading on the electrode coating rather than internal geometry. We use it at-line to confirm that cathode mass loading stays within a tight band, typically plus or minus 1.5 percent in a stable process. It answers a different question than radiography, but the two belong in the same quality plan: XRF keeps the coating correct, while X-ray and CT confirm the coated layers were assembled correctly.
Setting Scan Parameters on the Line
There is no universal setting, and anyone who claims otherwise has probably only run one cell format. Tube voltage sets penetration. For an aluminum-shelled semi-solid cell we often work in the 40 to 90 kilovolt range; thicker steel fixtures or dense tab assemblies may need more. Tube current and exposure time trade off against detector noise. Push them too far and you blur a moving cell; cut them too much and the image is too noisy for the algorithm to segment layers.
Geometry matters as much as the source. A larger source-to-detector distance sharpens edges but reduces magnification, so we tune it against the smallest defect we care about. For semi-solid cells I set the acceptance threshold from a validated sample set rather than a textbook number. Build that set by intentionally making cells with known misalignment, a known fold, and a known inclusion, then scan them until the image signature is unambiguous. Only then do you have a threshold that survives an audit. We also rescan a golden sample at the start of every shift to catch detector drift before it produces false rejects.
Turning Images into a Release Decision
An image is not a decision. The value comes from connecting what the scan finds to a documented rule. We record the scan ID, cell serial number, defect class, and measured dimension for every rejection, then review the distribution weekly. If misalignment drifts in one direction over several lots, that is a stacking fixture problem, not an inspection problem. Catching that trend is the real return on the equipment.
These checks also support the compliance story. UN 38.3 transport testing and IEC 62619 for industrial cells require evidence that the cells shipped match the design that was qualified. Internal inspection records are part of that evidence trail, because they show no foreign material or assembly defect slipped into the qualified population. For portable packs, IEC 62133-2 applies instead. And when a shipment moves by air, the airline and regulators under FAA and EASA rules rely on the UN 38.3 test summary; a clean inspection history strengthens the confidence behind that document. I keep scan records with the lot file so a customer or auditor can see exactly what left the line.
FAQ
What defects can X-ray inspection find in semi-solid cells?
It reliably finds tab misplacement, electrode stack misalignment, dense foreign particles, and gross voids. Paired with CT, it also localizes separator folds, internal pores, and wetting gaps. Electrical tests can miss many of these until capacity fades, which is why imaging is worth the investment.
How does CT differ from 2D X-ray for battery inspection?
2D radiography flattens the whole cell into one projection, which is fast but overlaps layers. CT reconstructs a three-dimensional volume from many projections, so you can slice through the stack, measure a void in place, and identify which layer contains a defect. We use 2D to screen and CT to diagnose.
What resolution is needed for semi-solid electrode inspection?
For practical line work, a CT voxel size around 30 to 80 micrometers resolves folds, voids, and separator movement in most pouch and prismatic semi-solid cells. Finer resolution is possible but raises scan time sharply, so match the voxel size to the smallest defect that changes a release decision.
Is X-ray inspection destructive to the cells?
No. A standard radiography or CT scan at diagnostic dose does not damage a lithium or semi-solid cell, so the inspected unit can still be used. That is why we can screen every cell in line and keep the golden sample in circulation for shift checks.
How much of production should be inspected?
I recommend 100 percent 2D screening for tab and alignment defects, plus a fixed CT sample each shift to verify the process baseline. Add full CT on any field failure. The exact sample size should follow your defect rate and customer requirements rather than a fixed rule.
What standards require battery internal inspection?
UN 38.3 covers transport qualification, IEC 62619 applies to industrial secondary cells, and IEC 62133-2 covers portable packs. None of them mandates a specific X-ray scan, but all depend on evidence that shipped cells match the qualified design. Inspection records are a strong part of that evidence and support the test summary used under FAA and EASA air transport rules.